Alumina Ceramic Sashin Kayan Wuta na Lantarki

Takaitaccen Bayani:

Alumina (AL2O3) yumbu ne na masana'antu wanda ke da tsayin daka, dogon sawa, kuma ana iya samuwa ta hanyar niƙan lu'u-lu'u.Ana ƙera shi daga bauxite kuma an kammala shi ta hanyar gyare-gyaren allura, latsawa, ƙwanƙwasa, niƙa, ƙwanƙwasa da aikin injina.


Cikakken Bayani

Tags samfurin

Filin Aikace-aikace

Alumina yumbu sassa wanda aka yadu amfani da lantarki aka gyara tare da high inji dukiya, high taurin, dogon sawa, babban rufi juriya, mai kyau lalata m, high zafin jiki resistant.

Alumina yumbu capacitors:Alumina yumbura suna da kyawawan kaddarorin dielectric kuma ana iya amfani da su don kera capacitors na yumbu.Wadannan capacitors suna da kwanciyar hankali mai kyau kuma suna iya aiki a cikin yanayi mai zafi kamar zafi mai zafi, matsa lamba, da zafi mai yawa, yana sa su yi amfani da su sosai a cikin na'urorin lantarki daban-daban.

Alumina yumbura marufi kayan:Alumina yumbura suna da kyakkyawan juriya na zafi, juriya na lalata, da juriya, kuma ana amfani da su sosai a cikin kayan marufi na semiconductor.Suna iya kare kwakwalwan kwakwalwar semiconductor yadda ya kamata daga tsangwama da lalata muhalli na waje, da inganta kwanciyar hankali da amincin na'urorin semiconductor.

A cikin kalma, sassan yumbura na alumina suna da aikace-aikace masu yawa a cikin kayan lantarki kuma suna taka muhimmiyar rawa.Tare da ci gaba da ci gaba da fasaha, aikace-aikacen yumbura alumina a cikin kayan lantarki zai ci gaba da fadadawa da zurfafawa.

Cikakkun bayanai

Yawan bukata:1pc zuwa miliyan 1 inji mai kwakwalwa.Babu iyaka MQQ.

Misalin lokacin jagora:kayan aikin kayan aiki shine 15days+ samfurin yin kwanaki 15.

Lokacin jagoran samarwa:15 zuwa 45days.

Lokacin biyan kuɗi:bangarorin biyu suka tattauna.

Tsarin samarwa:

Alumina (AL2O3) yumbu ne na masana'antu wanda ke da tsayin daka, dogon sawa, kuma ana iya samuwa ta hanyar niƙan lu'u-lu'u.Ana ƙera shi daga bauxite kuma an kammala shi ta hanyar gyare-gyaren allura, latsawa, ƙwanƙwasa, niƙa, ƙwanƙwasa da aikin injina.

Bayanan Jiki & Chemical

Alumina Ceramic(AL2O3) Takardun Magana
Takaddama naúrar Darasi A95% Darasi A97% Darasi A99% Darasi A99.7%
Yawan yawa g/cm3 3.6 3.72 3.85 3.85
Mai sassauƙa Mpa 290 300 350 350
Ƙarfin matsi Mpa 3300 3400 3600 3600
Modulus na elasticity Gpa 340 350 380 380
Juriya tasiri Mpm1/2 3.9 4 5 5
Weibull modulus M 10 10 11 11
Vickers hardulus Hv0.5 1800 1850 1900 1900
Ƙididdigar Ƙarfafawar thermal 10-6k-1 5.0-8.3 5.0-8.3 5.4-8.3 5.4-8.3
Ƙarfafawar thermal W/Mk 23 24 27 27
Juriya na girgiza thermal △T℃ 250 250 270 270
Matsakaicin zafin amfani 1600 1600 1650 1650
Volume resistivity a 20 ℃ Ω ≥1014 ≥1014 ≥1014 ≥1014
Dielectric ƙarfi KV/mm 20 20 25 25
Dielectric akai-akai εr 10 10 10 10

Shiryawa

Mu yawanci muna amfani da kayan kamar su tabbatar da danshi, tabbacin girgiza don samfuran da ba za su lalace ba.Muna amfani da jakar PP da kwandon katako na katako bisa ga buƙatun abokin ciniki.Ya dace da sufurin teku da na iska.

Jakar nailan
tire na katako
Karton

  • Na baya:
  • Na gaba:

  • Ku rubuta sakonku anan ku aiko mana